耐酸胶泥的施工方法:
1
、砌筑前应保证粘结砌筑面清洁干净。
2
、砌筑应连续在砌筑粘结打刮均匀拌和好的胶料,并通过揉挤使灰缝充浆饱满均匀。砌筑时灰缝刮平,不
勾缝。灰缝保持
3-5mm
。
3
、初凝变稠或凝结后的胶料不得破碎再用。
4
、在普通水泥砂浆、砼或钢基层上用本品时,应设隔离层.
5
、自然干养护,不得淋水、用水刷洗或与水蒸气接触
耐酸胶泥的施工方法: 1、砌筑前应保证粘结砌筑面清洁干净。 2、砌筑应连续在砌筑粘结打刮均匀拌和好的胶料,并通过揉挤使灰缝充浆饱满均匀。砌筑时灰缝刮平,不勾缝。灰缝保持3-5mm。 3、初凝变稠或凝结后的胶料不得破碎再用。 4、在普通水泥砂浆、砼或钢基层上用本品时,应设隔离层. 5、自然干养护,不得淋水、用水刷洗或与水蒸气接触
Construction method of acid proof daub: 1. Ensure the bonding and masonry surface clean and clean before masonry. 2, masonry should be continuous in the masonry, bonding, scraping, even mixing of good glue, and through kneading and squeezing to make the white seam filling uniform. Masonry mortar scraping, not pointing. The seam remains 3-5mm. 3, the initial thickening or condensation of the rubber may not be broken again. 4, in ordinary cement mortar, concrete or steel grassroots use this product, should be set isolation layer.5, natural dry maintenance, not water, water scrubbing or contact with water vapor