| 防腐耐酸胶泥使用注意事项 |
| 添加时间:2017/12/19 17:43:46 浏览次数: |
1、胶泥使用一般为砌筑法,要求灰缝均匀,浆缝密实,砌筑过程中不允许用水稀释。
1, the use of mud is usually masonry, which requires uniform seam, dense slit, and no water dilution in the process of masonry.
2、该产品保质期为九个月。
2. The warranty period of the product is nine months.
3、该产品在运输时严禁使用钩搭,不得摔扔,防止包装破裂混入杂质或受潮变质。
3, the product is strictly prohibited to use hook, not to throw, to prevent the breakage of packaging into impurities or dampness deterioration.
4、在储存、运输、保管过程中,保持干燥通风,粉料切勿雨淋受潮。
4. In the process of storage, transportation and storage, keep dry and ventilated, and the powder must not be wet and damp.
5、配制胶泥时,所用的工具要洁净,不要把用剩的胶泥硬块混入下次调合的胶泥中。
5, preparation of clay, using the tools should be clean, don't put the leftover Clay Lumps into next blending mortar. |
| 上一页 KPI耐酸胶泥施工方法 |
| 下一页 耐酸胶泥的防腐性能 |
Copyright © 技术支持:遨游网络